Cream
COMPOUND Wt%
A. Water 84.5
Potassium Hydroxide (45%) 0.4
Cola®Fax CPE 1.0
Cola®Lipid ST 2.5
Germaben II-E 0.6
Titanium Dioxide 0.5
PROCEDURE:
Heat Part A with agitation to 60½oC. Separately heat Part B to 60½oC. Homogenize Part
B into Part A for a sufficient time to ensure good emulsification. Stir cool to 45½oC and
add fragrance.
225 Colonial Drive South Pittsburg, TN 37380 Ph: 423-837-8800 Fax: 423-837-3888