Академический Документы
Профессиональный Документы
Культура Документы
MATERIAL
Shell
ASME II Section D Material? ( Y or N ) Y
Material Name: ASTM SA/AS 1548 7-490 - Plate
Nozzle
ASME II Section D Material? ( Y or N ) Y
Material Name: ASTM SA-312 TP316L S31603 - Wld. pipe
Required minimum thickness of a seamless shell based on circumferential stress (UG XX)
Internal Design Pressure: P= 2.41 MPa
Inside Radius of the Shell: R= 584.20 mm
Joint Efficiency: E= 1.00
Maximum Allowable Stress Value at Design Temperature: SV = 117.90 MPa
Minimum required thickness of shell: tr = 12.11 mm
Required minimum thickness of the nozzle based on circumferential stress (UG XX)
Internal Design Pressure: P= 2.41 MPa
Inside Radius of the Nozzle: R= 107.00 mm
Joint Efficiency: E= 1.00
Maximum Allowable Stress Value at Design Temperature: SN = 117.90 MPa
Minimum required thickness of the nozzle: trn = 2.22 mm
SUMMARY OF RESULTS