Comparison Table of Main Specification

aa. Hot Rolled Steel - Forming & Drawing Quality


Europe U.K. France Germany Italy Spain Sweden Japan U.S.A. U.S.A.
Euronom 111 BS 1449 NFA 36/301 DIN 1614 UNI 5867 UNE 36-086/11 SIS JIS G3131 ASTM SAE
- HR15 0C - - - - - -
- HR14 - - - AP10 - A569 -
FeP10 HR4 1C - FeP10 - SPHC - 1010
FeP11 HR3 2C StW22 FeP11 AP11 SPHD - 1018
FeP12 HR2 - StW23 FeP12 AP12 - A621 1016
FeP13 HR1 3C StW24 FeP13 AP13 SPHE A622 1016(Al Killed)

bb. Hot Rolled Steel - High Strength Grades(Structual Quality)


Europe U.K. France Germany Italy Spain Sweden Japan U.S.A. U.S.A.
EN10025(1993) BS 4360 NFA 35/501 DIN 17100 UNI 7070 UNE 36-080/11 SIS JIS G3101 ASTM SAE
S185 (BS 1449) 34/20 A34-2 - Fe320 A330 - SS34 A283B -
S235 40A - - - A370 14-13-12E - A283C -
S235/JR 40B E24-2 St37-2 Fe360B - - - - 1010
S275 43A - - - - 14-13-12E - A570Gr40 1018
S275JR 43B E28-2 St44-2 Fe430B - - - - 1016
- (BS 1449) 43/25 - - - - - S41 A36/A283D 1016(Al Killed)
S335 50A - - - A450 14-21-72 S60 A572Gr50 -
S335JR 50B - - Fe510B - - - - -
S335JO 50C E36-3 St52-3 Fe510C - - - - -

cc. Cold Rolled(Reduced) Steel - Forming & Drawing Quality


Europe U.K. France Germany Italy Spain Sweden Japan U.S.A. U.S.A.
EN10130(1991) BS 1449 NFA 36/401 DIN 1623 UNI 5866 UNE 36-086 SIS JIS G3141 ASTM SAE
FeP01 CR4 C St12 FeP01 AP01 14-11-42 SPCC A366 1010
FeP03 CR3 E RRSt13 FeP02 AP02 - SPCD - 1008
- CR2 - - - AP03 14-11-46 SPCE A619 1006
FeP04 CR1 ES RRSt14 FeP04 AP04 14-11-47 SPCEN A620 1006(Al Killed)
FeP05 - - - - - - - -
FeP06 - - - - - - - -

=> Surface Finish


A GR(General Purpose) X 3 MA X - - CLASS2
B FF(Full Finish) Z 5 MB Z - - CLASS1
dd. Hot Dipped Galvanized(Zinc-Coated) Steel - Forming & Drawing Quality
Europe U.K. France Germany Italy Spain Sweden Japan U.S.A. U.S.A.
EN 10142(1991) ASTM ASTM
BS 2989 NFA 36/321 DIN 17162 UNI 5753 UNE 36-310 SIS JIS G3302
(EN DIN/EN BS) (OLD) (AMENDMENT)
- Z1 - - FeO0GZ - - SGCC A526 A653-CQ
DX51D+Z/ZF/FeP02G Z2 GC St02Z FeKPGZ GRADE 41 14-11-51 SGCD1 A527 A653-LFQ
DX52D+Z/ZF/FeP03G Z3 GE St03Z FeP01GZ GRADE 43 14-11-52 SGCD2 A528 A653-DQ
DX53D+Z/ZF/FeP05G Z5 GES St05Z FeP03GZ GRADE 44 14-11-57 SGCD3 A642 A653-DDQ
DX54D+Z/ZF/FeP06G - - - - - - - -

ee. Hot Dipped Galvanized(Zinc Coated) Steel - High Strength Grades(Structual Quality)
Europe U.K. France Germany Italy Spain Sweden Japan U.S.A. U.S.A.
EN 10147(1992) BS 2989 NFA 36-322 DIN 17162 UNI 5753 UNE 36-310 SIS JIS G3302 ASTM A446 ASTM A653
S220GD+Z/ZF 300 Z22 C230 - Fe34GZ - - 245 SGC340 310 Gr-A 230 Gr.33
S250GD+Z/ZF 330 Z25 C250 StE250Z Fe37GZ - 14-12-70 360 Gr-B 255 Gr.37
S280GD+Z/ZF 360 Z28 C280 StE280Z Fe42GZ - 14-12-60 295 SGC400 380 Gr-C 275 Gr.40
S320GD+Z/ZF 390 - - - - - - 335 SGC440 450 Gr-D 345 Gr.50 Class 1
S350GD+Z/ZF 420 Z35 C350 StE350Z - - 12/22/1914 365 SGC490 570 Gr-E 550 Gr.80
S550GD+Z/ZF 560 Z55 C550 - - - - 560 SGC570 480 Gr-F 345 Gr.50 Class 3
EN(SAME SPEC) ; S220GD+Z./ZF = FeE220G / S250GD+Z/ZF = FeE250G / S280GD+Z/ZF=FeE320G / S320+Z/ZF=FeE320G / S350GD+Z/ZF=FeE350G / S550GD+Z/ZF=FeE550G

YS TS YS TS YS TS
=> Surface Finish
Europe U.K. France Germany Italy Spain Sweden Japan U.S.A. U.S.A.
EN 10142/147 BS 2989 NFA 36-321/322 DIN 17162 UNI 5753 UNE 36-310 SIS JIS G3302 ASTM A146 SAE
NA Spangle N NA NA Spangle N N Regular Spangle Regular Spangle -
MA Minimum Spangle M MA MA Minimum Spangle M M Minimized Spangle Minimized Spangle -
MB Smooth B B Skin Passed S S Skin Passed -
MC Extra Smooth XS C C - E - - - -
RA Regular - R(1Z) RA RA - - - - Regular -
RB Smooth - S(1Z) RB RB - - - - - -
RC Extra Smooth XS (1Z) RC RC - - - - - -
=> Coating Thickness
Europe U.K. France Germany Italy Spain Sweden Japan U.S.A. ZINC THICKNESS
EN 10142/147 BS 2989 NFA 36-321/322 DIN 17162 UNI 5753 UNE 36-310 SIS JIS G3302 ASTM A146
ZF100 IZ 100 (100g/sqm.) Z/100 - - Zf100. - - -
- IZ 180 (180g/sqm.) Z/180 - - Zf180 - - -
ZF140 - - - - - - - -
Z100 G100(100g/sqm.) Z100 100 Z100 Z100 Z100 Z12(120g/sqm.) G40 0.026
Z140 - - - - - - - -
Z200 G200(200g/sqm.) Z200 200 Z200 Z200 Z200 Z18(180g/sqm.) G60 0.034
Z225 - - - - - - Z22(220g/sqm.) G70 0.043
Z275 G275(275g/sqm.) Z275 275 Z275 Z275 Z275 Z27(270g/sqm.) G90 0.054
Z350 G350(350g/sqm.) Z350 350 Z350 Z350 Z350 Z35(350g/sqm.) -
Z450 G450(450g/sqm.) Z450 450 Z450 Z450 - Z45(450g/sqm.) -
Z600 G600(600g/sqm.) Z600 600 Z600 Z600 - Z60(600g/sqm.) -

ff) Electro Galvanized


Europe Europe France Germany Italy Spain Sweden Japan U.S.A. U.S.A.
EN 10152 EN 10152-92 DIN 17163-88 UNI 5753 UNE 36-310 SIS JIS G3313 ASTM A146 SAE
DC01+ZE Fe P01 ZE St 12 ZE SECC A591-CQ -
DC03+ZE Fe P03 ZE RRSt 13 ZE SECD A591-DQ -
DC04+ZE Fe P04 ZE St 14 ZE - -
DC05+ZE Fe P05 ZE - SECEN A591-DQSK -
DC06+ZE Fe P06 ZE - - - -

=> Coating Thickness(EG)


Nominal Minimum Zinc Thickness
MARKING
oz/sqf g/sqm g/sqm mic mtr mm(one side)
0.01/0.01 05/05 2.5 0.7 0 EB
0.03/0.03 10/10 8.5 1.4 0.001 E8
0.06/0.06 20/20 17.0 2.8 0.003 E16 ZE25/25
0.09/0.09 30/30 25.5 4.2 0.004 E24 ZE50/50
0.12/0.12 40/40 34.0 5.6 0.005 E32
0.14/0.14 45/45
0.15/0.15 50/50 42.5 7 0.006 E40 ZE75/75
0.17/0.17 55/55
0.18/0.18 60/60 51.0 8.5
70/70 59.5 9.9
80/80 68.0 11.3

New Amendments of EN Specification on Hot Dipped Galvanized Steel Sheet


1. EN10142(1991) ; zinc & iron-zinc alloy coatings - Forming Quality

Amendments Old Specification Quality


DX51D+Z, DX51D+ZF FeP02G Bending & Profiling Quality
DX52D+Z, DX52D+ZF FeP03G Drawing Quality
DX53D+Z, DX53D+ZF FeP04G Deep Drawing Quality
DX54D+Z, DX54D+ZF FeP05G Extra Deep Drawing Quality

2. EN10147(1992) ; zinc & iron - zinc alloy coating - Tensile Quality


Amendments Old Specification Quality
S220GD+Z / S220GD+ZF FeE220G Structural Quality Grade - A
S250GD+Z / S220GD+ZF FeE250G Structural Quality Grade - B
S280GD+Z / S220GD+ZF FeE280G Structural Quality Grade - C
S320GD+Z / S220GD+ZF FeE320G Structural Quality Grade - D
S350GD+Z / S220GD+ZF FeE350G
S550GD+Z FeE450G Structural Quality Grade - E
The Number incorporated in the grade specification of each EN10147(1992) - tensile quality - relates to the minimum
YIELD STRENGTH of the material.

Remarks
- In case of ASTM specification, the specification of Hot Dipped Galvanized Steel Sheet was unified as ASTM A653.
However, the former specifications likely to ASTM A526, A527, A528, A642 & A446 are also used and available.