Slag removal difficulties


d. Spatter

Submerged arc fluxes can be supplied in two forms. These are:


a. Sintered and agitated
b. Agitated and fused
c. Sintered and agglomerated
d. Fused and agglomerated

In submerged arc welding excessive arc voltage may cause:


a. Excessive penetration
b. Change in weld metal composition
c. Narrow weld width
d. Excessive bead profile

Slag inclusions would occur with:


a. Manual metal arc
b. Metal inert gas
c. Submerged arc welding
d. Both A and C

MMA

In MMA welding what parameter is used for control of penetration into the base material?
a. Voltage
b. Welding speed
c. Iron powders in the coating
d. Current

. In MMA welding, the slags produced can be varied to suit the welding position. Which type
of slag would be required for welding in the HV position?
a. Fluid
b. Viscous
c. Semi fluid
d. None of the above

The weld metal deposit of MMA electrodes achieves its mechanical strength through:
a. The core wire
b. The flux coating
c. Iron powders with the flux coating
d. None of the above

MMA electrodes can be grouped into three main types. These are:
a. Basic, cellulosic and rutile