Вы находитесь на странице: 1из 1

c. Spray transfer CO2 welding.

d. Basic coated MMA electrodes.


.

Submerged arc welds made with re-cycled flux are liable to:
a. Porosity.
b. Course grain size.
c. Undercut.
d. Incomplete penetration

In submerged arc welding the use of excessively high voltage would result in:
a. Insufficient flux melting
b. Excessive flux melting
c. Slag removal difficulties
d. Spatter

Submerged arc fluxes can be supplied in two forms. These are:


a. Sintered and agitated
b. Agitated and fused
c. Sintered and agglomerated
d. Fused and agglomerated

In submerged arc welding excessive arc voltage may cause:


a. Excessive penetration
b. Change in weld metal composition
c. Narrow weld width
d. Excessive bead profile

Slag inclusions would occur with:


a. Manual metal arc
b. Metal inert gas
c. Submerged arc welding
d. Both A and C

MMA

In MMA welding what parameter is used for control of penetration into the base material?
a. Voltage
b. Welding speed
c. Iron powders in the coating
d. Current

. In MMA welding, the slags produced can be varied to suit the welding position. Which type