Scope
This procedure address crack repair methods for Thinwall panels. All Thinwall cracks shall be
treated according to this procedure.
Repair Acceptance
Once cracks are repaired and cured, all repairs must be inspected by Quality Control and blue-
dotted prior to yarding the panel.
Depending on whether or not the crack is in the face, the rear or all the way through, the repair
procedure will differ. Refer to the applicable section(s) below.
Repair Procedure #1
Type 1 – Cosmetic Facial Crack (crack is .005” wide or less)
Patching material
Repair Procedure #1
Alternate (back-up) Procedure:
Use this procedure only when the use of flexible epoxy may aesthetically damage the face. This
alternate procedure shall only be used if the Project Manager, Yard Manager and QC Manager
agree that the default procedure cannot work with the desired result
Type 4 – Through Cracks (crack extends all the way through the facing concrete)
1. Handle facial panel cracks according to either the Type 1 or Type 2 procedure noted above
2. Handle rear panel cracks according to the Type 3 procedure noted above
Repair Procedure #1