Minimum Average Roll Values (MARV)

PROPERTY TEST UNIT CC4 CC4.5 CC6 CC7 CC8 CC10 CC12 CC16

Grab Tensile N 445 533 712 801 912 1112 1335 1691
ASTM-D4632
Strength (lb) (100) (120) (160) (180) (205) (250) (300) (380)

Elongation ASTM- D4632 % 50 50 50 50 50 50 50 50

CBR N 1112 1510 1824 2008 2224 3115 3510 4561


ASTM- D6241 (lb) (250) (340) (410) (450) (500) (700) (800) (1025)
Puncture
N 200 222 267 334 356 445 512 644
Trapezoidal Tear ASTM-D4533
(lb) (45) (50) (60) (75) (80) (100) (115) (145)
HYDRAULIC
Apparent mm 0.212 0.212 0.212 0.212 0.180 0.150 0.150 0.150
ASTM-D4751
Opening Size (US Sieve) (70) (70) (70) (70) (80) (100) (100) (100)

Permittivity ASTM- D4491 sec1 1.2 1.7 1.5 1.4 1.4 0.8 0.8 0.7

l/m/m2 5704 4485 4482 4278 3870 3056 2648 2037


Water Flow Rate ASTM-D4491
(gpm/ft2) (140) (120) (110) (105) (95) (75) (65) (50)
ENDURANCE
UV
ASTM- D4355 % @ 500 Hours 70 70 70 70 70 70 70 70
Resistance
PACKAGING

Roll Width Measured m (ft) 4.60 (15) 4.60 (15) 4.60 (15) 4.60 (15) 4.60 (15) 4.60 (15) 4.60 (15) 4.60 (15)

Roll Length Measured m (ft) 110 (360) 110 (360) 91 (300) 91 (300) 91 (300) 91 (300) 91 (300) 91 (300)

Note: Mullen Burst ASTM D4833 are no longer recognized by ASTM Committee D35 as an acceptable geotextile test method. Puncture Strength ASTM 4833 has been replaced with the Static (CBR)
Puncture ASTM D6241. For more information, refer to the ASTM website www.astm.org.
All values are MARV except where specified. All information and guidelines in this material is given in good faith but without warranty, expressed or implied with respect to the quality or fitness of the
products referred to herein for any particular purpose. Recommendations made herein refer to general use of Geotextiles. When non-standard conditions exist the company reserves the right to be
consulted prior to application. canadaculvert.com

Вам также может понравиться