Академический Документы
Профессиональный Документы
Культура Документы
WORK
INSTRUCTION WI/weld /09
Work Instructions for Carbon Impression Testing NO
Geometric changes: The electrode tip diameter will increase due to deformation and wear, such as mushrooming,
1.0 Purpose : pitting or local material removal by picking up.
Metallurgical changes: The material properties near the tip surface will also change during resistance welding such as
alloying with sheet and coating materials, and recrystallization and softening by overheating
3.0 Record:
Anti Spray : It is ideal compund for all ferrous parts . It is excellent corrosion resistance & useful aid to prevent flying metla
8.0 spraks form sticking to the metal thus avoiding further Grinding Deburring Operations
This is also suitable to useon welding gun nozzle which which will leave a film on a nozzle.this film prevents flying
metal sparks from sticking to the gun increses life of Gun
Directions Of Use
9.0
9.1 Refer Mfg Date of Mfg & ensures that date should not be more than 18 months
9.2 Shake can gently before use
9.3 Spray On the Gun Nozzle and inside the Nozzle over contact Tip before start of welding
9.4
Repeat the procedure after 4 Hours
10.0 CAUTION