(HARDENABILITY)
Myrna Ariati
Long 100 mm
Diameter 25,4 mm
Jominy Methodes
• Rod diameter is 1 in
• Put the standard sample at the Jominy equipment, which
at one side be cooled with water in jetspray .
• After high speed cooling, samples should be grinded in
one side, and the hardness measurement should be
done along the
• Samples should be cut in cross sectioned
• Make the relation between hardness and the distance
from the end quenched..
CCT dari
Jominy
Faktor-faktor yang mempengaruhi
hardenability
Langkah – langkah :
• Tentukan H: Table 4-4
• Tentukan Do : Figure 4-3
Jawab :
Calculation of Di ASTM standard A255
H = 0.4
Do = 0.9 in.
Tabel 4-4. Faktor “H” untuk
berbagai media quench.
Pengaruh Di dan H terhadap Do